Calcium-silicon alloy cored wire is made by using calcium-silicon alloy powder as the core material and wrapping it with a thin low-carbon steel strip. In the steelmaking process, this cored wire is fed into the ladle. After the outer steel strip melts in the high-temperature molten steel, the calcium-silicon alloy powder inside directly contacts the molten steel and undergoes a metallurgical reaction. Combined with argon stirring, this process efficiently achieves deoxidation, desulfurization, and inclusion removal in the molten steel, thereby significantly optimizing the overall quality and performance of the steel.
I. Product Definition and Basic Composition
1. Definition: Calcium silicon silicon alloy cored wire is a composite wire made by wrapping calcium silicon alloy powder with low-carbon thin steel strip using a core-wrapping machine. It is a key material in the ladle refining process of modern steel smelting and also a highly efficient deoxidizer and desulfurizer, widely used in the production of high-quality steel and special steel.
2. Composition: The core is a calcium silicon alloy powder core, and the outer layer is a thin steel strip. It is processed and shaped using specialized equipment to ensure the stable reaction of the core material with molten steel during the smelting process.
II. Core Metallurgical Functions
1. High-Efficiency Deoxidation: Ca in silicon-calcium alloys is a powerful deoxidizer, generating CaO in molten steel. This CaO then reacts with Al₂O₃ in the steel to form low-melting-point (1200-1400℃) calcium aluminate, which is easily floated and removed. When applied to Q345B steel, the deoxidation efficiency is 20-25% higher than that of silicon-aluminum-barium alloys, and the oxygen content in the steel can be reduced to below 20 ppm.
2. Deep Desulfurization: Ca has a very strong affinity for S, generating high-melting-point (2450℃) CaS. Furthermore, the solubility of CaS in molten steel at 1500℃ is only 0.0015%, resulting in a desulfurization efficiency of 40-50%, effectively reducing the sulfur content in the steel.
3. Inclusion Modification: Brittle Al₂O₃ inclusions in steel are converted into highly ductile calcium aluminates. For example, in bearing steel, this can refine inclusion size from 20 μm to below 5 μm, increasing the fatigue life of the steel by more than 30%.
4. Improved Steel Properties: This enhances the fluidity and castability of molten steel, reduces obstacles during the smelting process, and simultaneously improves the steel's plasticity, impact toughness, and optimizes casting and machining performance.
III. Advantages Compared to Traditional Processes
1. High Element Recovery: The wire feeding method allows the wire to directly react deep within the molten steel, preventing premature oxidation and loss of calcium in the slag layer. This significantly improves calcium recovery, far exceeding the yield of directly adding bulk silicon-calcium alloy (traditional bulk alloy calcium recovery is only 1-3%).
2. Minimal Disturbance to Molten Steel: Compared to bulk alloy addition and powder injection methods, this method reduces steel splashing and air intake, ensuring a stable smelting process.
3. Better Temperature Drop Control: After implementation, the temperature drop in molten steel is only 5-7℃/min, 3-6 times lower than traditional methods, which helps maintain the required temperature for the molten steel.
4. Precise Composition Adjustment: The feeding amount can be precisely controlled according to the content of elements such as aluminum and sulfur in the molten steel, allowing for fine-tuning of the chemical composition to meet the stringent composition requirements of high-end steel grades.
5. Economic and Environmentally Friendly: This method reduces equipment investment and operating costs, minimizes alloy loss, improves element utilization, and the wire feeding process is well-sealed, reducing dust and flue gas emissions, meeting the requirements of green production.
6. Improved smelting efficiency: It can shorten smelting time, increase the steel qualification rate, and help enterprises improve production efficiency.
IV. Application Scenarios
1. Primarily used in steelmaking and cast iron production, playing an irreplaceable role, especially in the production of low-sulfur steel, clean steel, high-strength steel, and special alloy steel.
2. Can completely replace aluminum final deoxidation, adaptable to ladle refining, continuous casting, and other processes, meeting the needs of the steel industry's development towards high-end and green technologies.